Uchungechunge lukapende olusindayo lwe-anti-corrosion lodonga lwangaphakathi lwamathangi okugcina uphethiloli asekelwe emanzini
Ukusebenza okufanayo
Ikhono elihle le-anti-corrosion ukuze lihlangabezane nezidingo zokuvikela zayo yonke i-coating;
Azikho izinto ezinobuthi neziyingozi ezikhiqizwa endaweni yokusabalalisa, inqubo yokwakha kanye nenqubo yokwenza ifilimu yokumboza, ehlangabezana nezidingo zokuvikelwa kwemvelo;ukwakheka okukabili, ubulukhuni obuhle, ukunamathela okuhle, ukumelana nowoyela ahlukahlukene, nokumelana okuhle kwamakhemikhali;
Ukufanisa kuhle, ifilimu yokugqoka ihlanganiswe ngokuqinile ne-substrate yensimbi, engathuthukisa ukunamathela kwefilimu yokugqoka ephezulu;ukwakhiwa ethangini kungakhuphula ngokufanelekile i-voltage yokukhanyisa ngaphandle kwezingozi zomlilo futhi kuqinisekise ikhwalithi yokwakha.
Ibanga lohlelo lokusebenza
Imikhiqizo engaconductive ifanele ukuvikela ukumbozwa kwezingxenye ezingadingi ugesi omile, njengamathangi kawoyela ongahluziwe nophahla oluntantayo.
Ukuvikelwa kwe-coating yodonga lwangaphakathi lwamathini, njll. Imikhiqizo ye-conductive ifaneleka odongeni lwangaphakathi lwamathangi okugcina amafutha aphelile (i-diesel, i-parafini, i-oli eguquguqukayo, i-petroli ehlukahlukene, njll.)
Ukwelashwa kwendawo
Zonke izindawo okufanele zigcotshwe kufanele zingabi nawoyela nothuli futhi kufanele zigcinwe zihlanzekile, zomile futhi zingangcoli futhi zonke izindawo kufanele zihlolwe futhi ziphathwe ngokuvumelana ne-ISO8504:1992.Kudingeka ukuthi ufinyelele izinga le-Sa2.5, futhi i-primer kufanele isetshenziswe kungakapheli amahora angu-6 ngemva kokuqhunyiswa kwesihlabathi.
Incazelo Yokwakha
Ukufafaza okungenamoya okucindezelayo okuphezulu kunconywa ukuthola umfaniswano kanye nefilimu enhle.
Hlanganisa ngokulinganayo ngokwesilinganiso.Uma i-viscosity ikhulu kakhulu, ingahlanjululwa ngamanzi ku-viscosity yokwakha.Ukuze kuqinisekiswe ikhwalithi yefilimu kapende, sincoma ukuthi inani le-dilution libe ngu-0% -5% wesisindo sokuqala sikapende.Umswakama ohlobene ungaphansi kwama-85%, futhi izinga lokushisa endaweni yokwakha likhulu kuno-10°C futhi likhulu kunezinga lokushisa lamazolo ngo-3°C.
Amaphakheji anconyiwe
I-non-conductive electrostatic support primer FL-2018D epoxy primer esekwe emanzini izikhathi ezi-3
I-Topcoat FL-2018M i-epoxy topcoat esekwe emanzini izikhathi ezi-4, ugqinsi oluhambisanayo alukho ngaphansi kuka-350μm
I-Static conductive esekela i-primer FL-2019D esekwe emanzini i-epoxy electrostatic conductive primer izikhathi ezi-2
I-Topcoat FL-2019M yamanzi esekelwe epoxy electrostatic conductive topcoat izikhathi ezi-3, ukushuba okuhambisanayo akukhona ngaphansi kuka-250μm.
Izinga eliphezulu
I-GB/T50393-2017
Ukusekela imingcele yezobuchwepheshe yokwakha
Isikhathi sokumisa (25℃) | indawo yomile≤4h, yomile kanzima≤24h |
Isikhathi sokuhlanganisa (25℃) | ubuncane obungu-4h, ubuningi obungu-7d |
Ukuvumelana nezimo mm | 1 |
Ukumelana namanzi ashisayo angama-90-100 ℃ | 48h |
Ukumelana nobuso (upende oqhubayo) | 108-1011 |
I-H2S, ukumelana ne-Cl-corrosion (1%) | 7d akukho okungajwayelekile |
Ukumelana ne-Acid (ifakwe ku-5% isixazululo se-H2SO4 sama-30d) | alukho ushintsho |
Ukumelana nowoyela (ucwiliswe ku-97# uphethiloli we-30d) | alukho ushintsho |
Okuqukethwe okuqinile | 58-62% |
Isikhathi sokusebenzisa esixutshiwe (25℃) | ≥4h |
Ibanga lokunamathela (indlela yombuthano). | 1 |
Ukuqina (ukuqina kwepensela) | ≥HB |
Amandla we-powder electrode esebenzayo (v) | 0.1 |
Ukumelana nomthelela Kg.cm | ≥50 |
Ukumelana namanzi anosawoti (okucwiliswe ku-5%NaCl isisombululo se-30d) | alukho ushintsho |
Ukumelana ne-alkali (okucwiliswe kusixazululo se-5% NaOH se-30d) | alukho ushintsho |